亚洲综合色精品乱_A级黄 毛视频免费看_亚洲女人天堂网在线_妞干在线观看_无码精品一区二区在线视频_国产呦萝免费视频_欧美一级无毛_亚洲熟女少妇av麻豆_影音先锋乱伦AV_国产超碰国产馆AV

Wuxi Precision Casting Factory home, welcome to visit Wuxi Yongsheng Metals Goods Co.,Ltd.!

Favorite | Problem | Sitemap

page_banner

Yong Sheng Metal Products

Piston Ring
Mechanical parts casting
Valve Castings
Civil Hardware
Casting structure
Automotive Castings
Workpiece
Auto parts casting
Structural precision casting
Civil metal casting
Valve class Precision Castings
Mechanical parts casting
Hardware
Automotive Parts Casting
Casting structure
Civil metal casting
Precision Casting Valve Parts
Mechanical parts casting
Valve, pump class
Auto parts casting
Structural precision casting
Civil metal casting
Precision Casting Valve Parts
Mechanical parts casting

Contact Us

Contact: Zhiyong,Lu

Hotline:86- 13806173867
Contact: Miss Ma

Tel: 0510-68916532
Fax: 0510-68916533
E-mail: lyzz@vip.163.com 
caochuantou@163.com

Website: http://vistasp2.cn

Address: No. 38 Xiqun Meicun Industrial Park Road, Wuxi


Civil HardwareMore>>

Machinery parts precision castings

Publisher: Wuxi Yongsheng Metals Goods Co.,Ltd. Release Time:2015/10/15 20:03:48 Clicks:1893 Close
Product Details
Sol casting procedures
1, inspection equipment, temperature control instrumentation is in normal working condition.
2, dewaxing autoclave recycling old wax was poured into the filter tank filter; and then sent to stand in the bucket, less than 90 ℃ under the standing 6-8h.
3, after completion of the precipitation standing water off the wax was poured except bucket.
4, in addition to a bucket of wax, heat and stirred at 110-120 ℃, the residual moisture evaporation, the visual surface without foam until the liquid wax.
5, the finished wax liquid water, after <60 mesh filter and then into the <standing barrel 90 ℃, the insulation was allowed to stand for more than 12h.
6, all except bucket, standing barrel should regularly let go of residual water and debris in the bottom of the dirt.
7, the bucket standing good recovery process liquid wax to the die press machine cooler in wax for the main production die (runner).
8, under the old wax material performance and the wax material consumption, from time to time in the right amount standing bucket II add a new wax, generally about 3% -5%.
9, the qualified incubator poured liquid wax wax cylinders, to reduce the liquid wax wax cylinder gas, first for a period of time after a high temperature 80 ℃ / 2h dropped to 54 ℃. At 54 ± 2 ℃ incubation 24h, before the wax mold for pressing.
About Us

Wuxi Yongsheng Metals Goods Co.,Ltd.

Hotline:86-13806173867

Contact: Zhiyong Lu
Contact: Miss Ma

Tel: 0510-68916532
Fax: 0510-68916533
E-mail: lyzz@vip.163.com

 caochuantou@163.com

Website:http://vistasp2.cn

Address: No. 38 Xiqun Road Industrial Park, Jiangsu Wuxi Meicun

Order online
Ordering Products: 
Contact: 
Tel: 
Address: 
Email: 
Remarks: 
Code:  3767
  
Related Products
????

QQ??????

  • Customer Advisory
  • ??????????????
  • ??????????????
  • Technical consulting
  • ??????????????
Click to hide